Polymer Property : Tensile Strength at Break = 125.6 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 125.6 MPa
18220 psi
ASTM D3759
3M 8421 Polyester Tape
3M™ Polyester Tape 8421 is for photographic industry for splicing most film for processing through the developing chemicals.Information provided by 3M
Tensile Strength at Break 125.6 MPa
18220 psi
ASTM D3759
3M 8422 Polyester Tape
3M™ Polyester Tape 8422 is for photographic industry for splicing most film for processing through the developing chemicals.Information provided by 3M