Polymer Property : Tensile Strength at Break = 125000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 862 MPa
125000 psi
Hard
California Fine Wire Alloy 20-245 Precious Metal Alloy
All values may vary dependent on specific design and usageProprietary compositionCapabilities: WireInsulatedInformation provided by California Fine Wire.
Tensile Strength at Break 862 MPa
125000 psi
Hard
California Fine Wire Dumet Nickel Iron Core Copper Clad Alloy
All values may vary dependent on specific design and usage99.9% copper cladding over iron-nickel coreCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Tensile Strength at Break 862 MPa
125000 psi
Hard
California Fine Wire Nickel 271 Super Alloy
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Tensile Strength at Break 862 MPa
125000 psi
Hard
California Fine Wire Nickel 272 Super Alloy
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.