Polymer Property : Tensile Strength at Break = 13.4741 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 13.4741 MPa

@Temperature 85.0 °C,
Time 605000 sec
1954.26 psi

@Temperature 185 °F,
Time 168 hour
Heat Aging; ISO 188, Method B
S&E Specialty Polymers TufTech™ SE11-023E PVC Compound
Application: Automotive – PVC, black, exterior weatherable, elastomeric, extrusion molding compound.Information provided by S&E Specialty Polymers