Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 14.21 MPa @Temperature 100 °C, Time 605000 sec |
2061 psi @Temperature 212 °F, Time 168 hour |
After Dry Heat Aging; ASTM D865 |
Seals Eastern 7272 Butyl and Halobutyl Rubber General purpose Chlorobutyl; High dampingInformation provided by Seals Eastern, Inc. |