Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 14.39 MPa | 2087 psi | After 7 days at 125°C; ASTM D573 |
Advanced Polymer Alloys Alcryn® 2170 BK Melt Processable Rubber Alcryn 2100 Series melt-processable rubber (MPR) offer a broader range of bonding to rigid substrates while maintaining all the excellent performance features of traditional Alcryn. The 2100 grades.. |
|||
Tensile Strength at Break | 14.39 MPa | 2087 psi | After 7 days at 125°C; ASTM D573 |
Advanced Polymer Alloys Alcryn® 2180 NC Melt Processable Rubber Alcryn 2100 Series melt-processable rubber (MPR) offer a broader range of bonding to rigid substrates while maintaining all the excellent performance features of traditional Alcryn. The 2100 grades.. |