Polymer Property : Tensile Strength at Break = 14.56 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 14.56 MPa
2112 psi
Air at 275°F, 1008 hr; ASTM D573
ExxonMobil Santoprene® 221-87 Thermoplastic Elastomer  (discontinued **)
A hard, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide..