Tensile Strength at Break 14.9 MPa
2160 psi
Daikin DAI-EL G-783 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content
Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Features: Fast vulcanization, for complex shapes.Information provided by Daikin ..
Tensile Strength at Break 14.9 MPa
2160 psi
in Air 150°C, 168 hr; ASTM D573
ExxonMobil Santoprene® 201-87 Thermoplastic Elastomer
A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra..