Polymer Property : Tensile Strength at Break = 14870 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 102.5 MPa

@Temperature 160 - 175 °C,
Time 1.80e+7 sec
14870 psi

@Temperature 320 - 347 °F,
Time 5000 hour
5 [mm/min], 50% Loss of Tensile Strength; ICE 216
Akro-Plastic Akromid® B3 GF 40 (2474) PA 6 Dry, 40% Glass Filled
AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur..
Tensile Strength at Break 102.5 MPa

@Temperature 130 - 150 °C,
Time 7.20e+7 sec
14870 psi

@Temperature 266 - 302 °F,
Time 20000 hour
5 [mm/min], 50% Loss of Tensile Strength; ICE 216
Akro-Plastic Akromid® B3 GF 40 (2474) PA 6 Dry, 40% Glass Filled
AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur..
Copyright © lookpolymers.com All Rights Reserved