Mechanical Properties Metric English Comments
Tensile Strength at Break 15.97 MPa

@Temperature 125 °C,
Time 252000 sec
2316 psi

@Temperature 257 °F,
Time 70.0 hour
ASTM D412 Method A
Seals Eastern 7267 Ethylene-Propylene Rubber
EPDM for high temperature steam service. Also available as a Y267-Type (7267L).Information provided by Seals Eastern, Inc.