Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | >= 10.78 MPa | >= 1564 psi | ASTM D412 Method A |
Seals Eastern 5724 Fluorocarbon-Elastomer Formulated Viton®. General service.Information provided by Seals Eastern, Inc. |
|||
Tensile Strength at Break | 10.78 MPa | 1564 psi | |
Shin-Etsu Silicones X-30-1028U Low Temperature Silicone Elastomer ShinEtsu X301028U is a phenyl (PVMQ) silicone base. This product is designed for good low temperature characteristics. Product Features: A broad range of service temperatures from 100 to +260°C (.. |