Mechanical Properties Metric English Comments
Tensile Strength at Break 17.25 MPa
2502 psi
ASTM D412
Borealis FR4832 Chemically Crosslinkable Polyethylene Compound for Primary Automotive Wires
FR4832 is a Chemically Crosslinkable Polyethylene Compound for Primary Automotive Wires. Applications: FR4832 is intended for use as a 125º C rated primary insulation for crosslinked automotive wi..