Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 10.1 - 11.7 MPa | 1470 - 1700 psi | |
Plastic Lumber from the Plastic Lumber Co. Description: Plastic Lumber is a product similar to wood that is made from recycled plastic jugs. Products will never splinter, rot, crumble or need painting. Plastic Lumber has rapidly gained accep.. |