Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 11.9 MPa
1720 psi
Data derived from Type IV specimen, 75 mil plaques, @ 20" min.; ASTM D638
LyondellBasell Petrothene® NA143063 Low Density Polyethylene
ApplicationsPETROTHENE NA 143 is a series of homopolymer resins for blown film. Applications include stiff liners. Regulatory StatusNA 143 meets the requirements of the Food and Drug Administration..
Tensile Strength at Break 11.9 MPa
1720 psi
Indium Corp. Indalloy 1 Indium-Tin Solder Alloy
Fair wettability on glass, quartz, and many ceramics. Good low temperature malleability. Compensates for some CTE mismatch. Low vapor pressureInformation Provided by Indium Corporation
Tensile Strength at Break 11.9 MPa
1720 psi
Across flow; ASTM D412
ExxonMobil Santoprene® 8271-80HT Thermoplastic Rubber  (discontinued **)
Description: A colorable thermoplastic elastomer which complies with FDA regulations for rubber articles intended for repeated use. It can be processed using injection molding or extrusion melt pro..