Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 18.3 MPa | 2650 psi | 510 mm/min; ASTM D412A |
PolyOne Geon™ Vinyl Flexible XV3901 Polyvinyl Chloride, Flexible (PVC, Flexible) All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high .. |
|||
Tensile Strength at Break | 18.3 MPa | 2650 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible 86155 Polyvinyl Chloride, Flexible (PVC, Flexible) 86155 is a flexible (90A durometer) vinyl compound formulated from FDA-santioned raw materials. This compound has received NSF Standard 61 only for sheets applications.NOTE: All ingredients used in .. |
|||
Tensile Strength at Break | 18.3 MPa | 2650 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible R5230C Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 18.3 MPa @Temperature 200 °C, Time 1.21e+6 sec |
2660 psi @Temperature 392 °F, Time 336 hour |
After Dry Heat Aging; ASTM D865 |
Seals Eastern 7145 Fluorocarbon-Elastomer FKM specially for oil & gas service.Information provided by Seals Eastern, Inc. |
|||
Tensile Strength at Break | 18.3 MPa | 2650 psi | ASTM D638 |
Teknor Apex APEX® 3611-75 Polyvinyl Chloride, Flexible Uses: Medical/Healthcare Applications Agency Ratings: NSF 61 Forms: Pellets Additional Information: Second Generation SeriesInformation Provided by Teknor Apex |
|||
Tensile Strength at Break | 18.3 MPa | 2650 psi | ASTM D638 |
Teknor Apex APEX® 80855 Polyvinyl Chloride, Flexible Notes: 90°C Insulation; RoHS CompliantFeatures: Sunlight Resistant (720 hours) Uses: Cable Jacketing; Insulation; Outdoor ApplicationsAgency Ratings: UL QMTT2 .E73402 Forms: Pellets Wire Types: T.. |
|||
Tensile Strength at Break | 18.3 MPa | 2650 psi | ASTM D638 |
Teknor Apex APEX® 4011 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
Tensile Strength at Break | 18.3 MPa | 2650 psi | ASTM D412 |
UBE UBEPOL BR153A Oil-Extended BR Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C) Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE. |
|||
Tensile Strength at Break | 18.3 MPa | 2650 psi | ASTM D412 |
Teknor Apex APEX® 2580-H Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Good FlexibilityUses-General Purpose, ProfilesAppearance-Natural Color, OpaqueForms-PelletsProcessin.. |
|||
Tensile Strength at Break | 18.3 MPa | 2650 psi | ASTM D638 |
Teknor Apex APEX® 3701-80NT Polyvinyl Chloride, Flexible Features: Non-DEHP Plasticizer; Ethylene Oxide Sterilizable; High Heat Resistance Uses: Medical/Healthcare Applications Processing Method: Extrusion Forms: PelletsInformation Provided by Teknor Apex.. |