Polymer Property : Tensile Strength at Break = 180.5 MPa
Polymer Property :
Tensile Strength at Break =
180.5 MPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
180.5
MPa
26180
psi
ASTM D3759
3M 3361 Stainless Steel Foil Tape
Corrosion resistantInformation provided by 3M