Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 12.6 MPa @Temperature 23.0 °C |
1830 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versaflex™ CL E90 Thermoplastic Elastomer (TPE) Versaflex™ CL E90 is an exceptional clarity, high performance and autoclavable solution ideal for healthcare and food packaging. Versaflex™ CL E90 is also formulated without the use of plasticizer.. |
|||
Tensile Strength at Break | 12.6 MPa | 1830 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible R355AM Polyvinyl Chloride + NBR (PVC+NBR) Information provided by PolyOne |
|||
Tensile Strength at Break | 12.6 MPa | 1830 psi | ASTM D1414 |
Greene Tweed CHEMRAZ® 653 Perfluoroelastomer Chemraz® is a black perfluoroelastomer specifically formulated to meet the extreme demands of diffusion, LPCVD and thin dry processing applications. It exhibits superior compression set resistan.. |
|||
Tensile Strength at Break | 12.6 MPa | 1830 psi | |
Taiwan PU Corporation UR80 Polyester Urethane Rubber UR80 is a polyester urethane rubber which is an easy to process millable gum especially developed for improved compounding and processing benefits. It can be processed and compounded by the use of .. |
|||
Tensile Strength at Break | 12.6 MPa | 1830 psi | ASTM D638 |
Teknor Apex APEX® 7500-70 Polyvinyl Chloride, Flexible Notes: 105°C General Purpose; RoHS Compliant Features: High Heat Resistance Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL.. |
|||
Tensile Strength at Break | 12.6 MPa | 1830 psi | ASTM D412 |
Teknor Apex Monprene® MP-1320E Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | >= 12.6 MPa | >= 1830 psi | Compounded, 35 mins.; ASTM D3185 |
Dynasol Solprene® 375 Solution Random SBR Solprene 375 is a tin coupled, random styrene-butadiene copolymer with 24% styrene content. It is extended with naphtenic oil. S-375 is used as ingredient in compounds for battery cases, tires, cabl.. |