Mechanical Properties Metric English Comments
Tensile Strength at Break >= 12.95 MPa
>= 1878 psi
ASTM D412 Method A
Seals Eastern 7272 Butyl and Halobutyl Rubber
General purpose Chlorobutyl; High dampingInformation provided by Seals Eastern, Inc.