Polymer Property : Tensile Strength at Break = 19.49 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 19.49 MPa
2827 psi
ASTM D412
DuPont Performance Polymers Kalrez® Spectrum™ 0090 Fluoroelastomer
DuPont™ Kalrez® 0090 perfluoroelastomer parts deliver durable, reliable sealing solutions for applications requiring excellent rapid gas decompression (RGD) properties as well as high hardness and..