Polymer Property : Tensile Strength at Break = 19.69 MPa
Polymer Property :
Tensile Strength at Break =
19.69 MPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
19.69
MPa
2856
psi
AVG; ASTM D412 Method A
Seals Eastern 5353 Nitrile Rubber
General purpose NitrileInformation provided by Seals Eastern, Inc.