Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 131.3 MPa | 19040 psi | ASTM D3759 |
3M 8412 Polyester Film Tape 3M™ Polyester Tape 8412 has excellent tensile strength and abrasion resistance, that can be used for many permanent edging and reinforcing types of applications.Information provided by 3M |