Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 199 MPa | 28900 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Nymax™ GF 1200 A 33 Natural Polyamide 66 (Nylon 66) The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil.. |
|||
Tensile Strength at Break | 199 MPa | 28900 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON RE0069S PA 66 LNP* STAT-KON* RE0069S is a compound based on Nylon 66 resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant, Heat Stabilized. |
|||
Tensile Strength at Break | 199 MPa | 28900 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP VERTON RX10409D PA 66 LNP* VERTON* RX10409D is a compound based on Nylon 66 containing proprietary fillers. Added feature of this grade is: Structural. |