Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength at Break = 2.10 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 2.10 MPa
305 psi
Die C; Flow direction; ASTM D412
Teknor Apex Sarlink® 3135 Thermoplastic Elastomer
A low hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3135 can be processed by injection molding or extrusion for ap..
Tensile Strength at Break >= 2.10 MPa
>= 305 psi
after aging, 7h, 110°C; IEC 60811-1-2
Borealis Casico™ FR6082 Reduced Fire Hazard Jacketing Compound
Casico™ FR6082 is a thermoplastic, reduced fire hazard, zero halogen black jacketing compound combined with high mechanical strength, toughness and excellent extrusion properties. It is based on th..
Tensile Strength at Break 2.10 MPa
305 psi
ASTM D412
3M 540 Polyurethane Sealant
3M™ 500-Series Polyurethane Construction Sealant, Polyurethane Sealant and Polyurethane Adhesive Sealant products are one component, moisture curing products which form permanent elastic bonds. The..
Tensile Strength at Break 2.10 MPa
305 psi
ISO 527-1
Barlog Plastics KEBAFLEX S 25 A.01 TPE-S, Shore A25, translucent
TPE-SInformation provided by BARLOG plastics GmbH.
Tensile Strength at Break 2.10 MPa
305 psi
ASTM D3759
3M 9343 Conformable Sound Management Film
3M™ Conformable Sound Management Film 9343 is designed for the reduction of noise, vibration, squeaks, and rattles in automotive interior applications. The currently available materials for these a..