Polymer Property : Tensile Strength at Break = 2039 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 14.06 MPa

@Temperature 121 °C,
Time 605000 sec
2039 psi

@Temperature 250 °F,
Time 168 hour
ASTM D638
LG Chemical LUTENE XL2700BK PE Compound
Description: LUTENE XL2700BK has excellent strippability, processability, weather resistance, heat resistance for medium and high voltage power cables. The advantage of LUTENE XL2700BK over conventi..