Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 21.2 MPa | 3070 psi | 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible A48248D Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 21.2 MPa | 3070 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible XV3581G Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 21.2 MPa | 3070 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible P484B Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 21.2 MPa | 3080 psi | ASTM D638 |
Teknor Apex APEX® 84854 Polyvinyl Chloride, Flexible Notes: 105°C Insulation; RoHS CompliantFeatures: Flame Retardant; High Heat Resistant Uses: InsulationAgency Ratings: UL 62 Forms: Pellets Wire Types: SJT; ST; SVTInformation Provided by Teknor A.. |
|||
Tensile Strength at Break | 21.2 MPa | 3070 psi | ASTM D3759 |
3M 3380 General Purpose Aluminum Foil Tape 40 lb natural kraft paper liner. Good for narrow slit rolls. UL 723 ClassifiedInformation provided by 3M |
|||
Tensile Strength at Break | 21.2 MPa | 3070 psi | ASTM D3759 |
3M 4380 General Purpose Aluminum Foil Tape 3M™ Aluminum Foil Tape 4380 is a general purpose aluminum foil tape offering a dead soft aluminum foil backing combined with an acrylic pressure sensitive adhesive.Information provided by 3M |
|||
Tensile Strength at Break | 21.2 MPa | 3070 psi | ASTM D3759 |
3M 4201 Lead Foil Tape Permanent acrylic adhesiveInformation provided by 3M |
|||
Tensile Strength at Break | 21.2 MPa | 3070 psi | Press Cure 10 Minutes @ 177°C, Post Cure 16 Hours @ 232°C; ASTM D412 |
3M Dyneon™ TFE 90Z Peroxide Cure Perfluoroelastomer 3M™ Dyneon™ Peroxide Cure Perfluoroelastomer PFE 90Z is a technically advanced peroxide curable perfluoroelastomer, designed to meet the challenges of demanding sealing applications. It is classif.. |