Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | >= 14.6 MPa | >= 2120 psi | |
Sibur SKN-18PVC-30 Nitrile-Butadiene Rubber (NBR) For production of rubber and asbestos technical articles which are used as sets for automobile, air planes, different machines and equipment, agricultural, drilling, and polygraph machinery, as well.. |
|||
Tensile Strength at Break | 14.6 MPa | 2120 psi | ASTM D412 |
Teknor Apex Telcar® TL-1190A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Strength at Break | 14.6 MPa | 2120 psi | ASTM D412 |
UBE UBEPOL BR130B Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C) Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE. |
|||
Tensile Strength at Break | 14.6 MPa | 2120 psi | |
Daikin DAI-EL G-701 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Features: General purpose with excellent compression set.Information provided by.. |
|||
Tensile Strength at Break | 14.6 MPa | 2120 psi | |
Daikin DAI-EL G-752 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Information provided by Daikin Industries. |