Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 22.75 MPa | 3300 psi | ASTM D1414, ASTM D412 |
DuPont Performance Polymers Kalrez® Spectrum™ 7090 Fluoroelastomer DuPont™ Kalrez Spectrum™ 7090 perfluoroelastomer parts are specifically targeted for use in applications requiring high hardness/higher modulus properties. These specialty black parts have excelle.. |