Mechanical Properties Metric English Comments
Tensile Strength at Break 15.21 MPa
2205 psi
JIS-K-6723
Denka VINYKON S3098 PVC, S grade for refrigerator gaskets
A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding..