Mechanical Properties Metric English Comments
Tensile Strength at Break 226 MPa
32800 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP ECL36XXQ PEI
LNP* Lubricomp* ECL36XXQ is a compound based on Polyetherimide containing 30% Carbon Fiber, 15% PTFE. Added features of this material include: Internally Lubricated.
Tensile Strength at Break 226 MPa
32800 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP RFN1ASXS PA 66 (Europe-Africa-Middle East)
LNP* Lubricomp* RFN1ASXS is a compound based on Nylon 66 resin containing Glass Fiber, MOS2. Added features of this material include: Heat Stabilized.
Tensile Strength at Break 226 MPa
32800 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP UX96507 PPA
LNP* LUBRICOMP* UX96507 is a compound based on PPA containing proprietary fillers. Added feature of this grade is: Wear Resistant.
Tensile Strength at Break 226 MPa
32800 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP UX96507 PPA
LNP* LUBRICOMP* UX96507 is a compound based on PPA containing proprietary fillers. Added feature of this grade is: Wear Resistant.