Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 1.59 MPa | 230 psi | ASTM D638 |
ExxonMobil Escorene® UL 7710 Adhesive Application Resin Escorene Ultra UL 7710 is a very high flow, 26.7% vinyl acetate copolymer that has very good compatibility with hydrocarbon and natural tackifiers and most waxes. It is suitable for making hot melt .. |
|||
Tensile Strength at Break | 1.59 MPa | 230 psi | ASTM D638 |
ExxonMobil Escorene® UL 7710E Adhesive Application Resin Escorene Ultra UL 7710E is a very high flow, 26.7% vinyl acetate copolymer that has very good compatibility with hydrocarbon and natural tackifiers and most waxes. It is suitable for making hot melt.. |