Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 160.5 MPa | 23280 psi | ASTM D3759 |
3M 5401 Traction Tape 3M™ Traction Tape 5401 is a single coated glass cloth tape with silicone coated backing used for wrapping rollers to provide traction and non-stick surface.Information provided by 3M |