Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 24.4 MPa | 3540 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible XV3859 Polyvinyl Chloride, Flexible (PVC, Flexible) All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high .. |
|||
Tensile Strength at Break | 24.4 MPa | 3540 psi | Tensile stress at break. |
Dow Pellethane® 2351-85AE Polyurethane Elastomer, Ether Based
(discontinued **) PELLETHANE® 2351-85AE elastomer is a polyether hybrid specialty polyurethane elastomer compound which combines excellent resistance to fuels and oils with good hydrolytic stability and high damping.. |