Polymer Property : Tensile Strength at Break = 24.7 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 24.7 MPa
3580 psi
510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible B7D01 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tensile Strength at Break 24.7 MPa
3580 psi
ASTM D638
LyondellBasell Plexar® PX2246 Extrudable Tie-Layer Resin - Anhydride Modified HDPE
General DescriptionPlexar® tie-layers are chemically modified resins used to bond unlike materials, primarily in packaging and industrial applications. Common adherents include polyethylene resin..
Tensile Strength at Break 24.7 MPa

@Temperature 145 °C,
Time 2100 sec
3580 psi

@Temperature 293 °F,
Time 0.583 hour
ASTM D412
LG Chemical SBR 1739 High Acrylonitrile Polymer
Description: SBR 1739 is an oil extended cold polymerization SBR with 37.5 parts of Low PCA (PolyCyclic Aromatic) oil and styrene-butadiene copolymer of 40% bound styrene. Raw materials for this p..
Tensile Strength at Break 24.7 MPa

@Temperature 145 °C,
Time 2100 sec
3580 psi

@Temperature 293 °F,
Time 0.583 hour
ASTM D412
LG Chemical SBR 1789 High Acrylonitrile Polymer
Description: SSBR 1789 is an oil extended cold polymerization SBR with 37.5 parts of Low PCA (RAE type) oil and styrene-butadiene copolymer of 40% bound styrene. Raw materials for this product are ..
Tensile Strength at Break 24.7 MPa
3580 psi
Transverse to Flow; ASTM D882
Diamond Polymers NPP10-0105 Vinyl Acetate Copolymer
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.