Mechanical Properties Metric English Comments
Tensile Strength at Break 251 MPa

@Temperature -40.0 °C
36400 psi

@Temperature -40.0 °F
ASTM Test
BASF Ultramid® TG7S 35% Glass Filled PA6 (Dry)
Ultramid TG7S is a 34% glass reinforced, heat stabilized, impact modified PA6 injection molding grade. It was developed to meet the demanding requirements of the first North American seat cushion ..
Tensile Strength at Break 251 MPa

@Temperature -40.0 °C
36400 psi

@Temperature -40.0 °F
ISO Data
BASF Ultramid® TG7S 35% Glass Filled PA6 (Dry)
Ultramid TG7S is a 34% glass reinforced, heat stabilized, impact modified PA6 injection molding grade. It was developed to meet the demanding requirements of the first North American seat cushion ..