Tensile Strength at Break 257 MPa
37300 psi
ASTM D638
SABIC Innovative Plastics LNP VERTON UV00AS PPA (Asia Pacific)
LNP* Verton* UV00AS is a compound based on Polyphthalamide resin containing Long Glass Fiber. Added features of this material include: Heat Stabilized.
Tensile Strength at Break 257 MPa
37300 psi
ASTM D638
SABIC Innovative Plastics LNP VERTON UV00ASU PPA
LNP* VERTON* UV00ASU is a compound based on Polyphthalamide resin containing 50% Long Glass Fiber. Added features of this material include: UV Stabilized, Heat Stabilized, Structural.
Tensile Strength at Break 257 MPa
37300 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP PX01658 PA 6
LNP* Thermocomp* PX01658 is a compound based on Nylon 6 containing Proprietary Fillers.
Tensile Strength at Break 257 MPa
37300 psi
ASTM D638
SABIC Innovative Plastics LNP VERTON UV00AS PPA
LNP* VERTON* UV00AS is a compound based on Polyphthalamide resin containing 50% Long Glass Fiber. Added features of this material include: Heat Stabilized, Structural.