Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 17.8 MPa | 2580 psi | ASTM D1414 |
Greene Tweed CHEMRAZ® 526 Perfluoroelastomer Greene Tweed’s Chemraz® 526, a perfluoroelastomer, offers superior chemical compatibility coupled with explosive decompression resistance, making it the ideal compound for fluid handling equ.. |
|||
Tensile Strength at Break | 17.8 MPa | 2580 psi | ASTM D638 |
Teknor Apex APEX® 6500-90 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
Tensile Strength at Break | 17.8 MPa | 2580 psi | ASTM D412 |
Teknor Apex MF 588 Polyvinyl Chloride, Flexible Film Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Film, Medical Applications Forms-PelletsInformation provided by Teknor Apex Company |
|||
Tensile Strength at Break | 17.8 MPa | 2580 psi | ASTM D638 |
Chesterton ARC 5 Paste grade Rapid Cure Abrasion Control Description: ARC 5 is an advanced composite formulated for emergency repair and patching of metal components subject to light abrasive and corrosive conditions. It can be used to seal leaks and patc.. |
|||
Tensile Strength at Break | 17.8 MPa | 2580 psi | ASTM D638 |
Chesterton MRS 5 Metal Rebuilding System MRS 5 is an advanced composite formulated for emergency repair and patching of metal components subject to light abrasive and corrosive conditions. It can be used to seal leaks and patch holes as we.. |