Tensile Strength at Break 180.83 MPa
26227 psi
ASTM D638
A. Schulman SCHULAMID® 6 GF33 33% Glass Fiber Reinforced Nylon 6
Information provided by A. Schulman.
Tensile Strength at Break 180.83 MPa
26227 psi
ASTM D638
A. Schulman SCHULAMID® 6 GF33 33% Glass Fiber Reinforced Nylon 6
Information provided by A. Schulman.
Tensile Strength at Break 180.83 MPa
26227 psi
ASTM D638
A. Schulman SCHULAMID® 6 GF33 33% Glass Fiber Reinforced Nylon 6
Information provided by A. Schulman.
Tensile Strength at Break 180.83 MPa
26227 psi
ASTM D638
A. Schulman SCHULAMID® 6 GF33 33% Glass Fiber Reinforced Nylon 6
Information provided by A. Schulman.
Tensile Strength at Break 180.83 MPa
26227 psi
ASTM D638
A. Schulman SCHULAMID® 6 GF33 33% Glass Fiber Reinforced Nylon 6
Information provided by A. Schulman.
Tensile Strength at Break 180.83 MPa
26227 psi
ASTM D638
A. Schulman SCHULAMID® 6 GF33 33% Glass Fiber Reinforced Nylon 6
Information provided by A. Schulman.
Copyright © lookpolymers.com All Rights Reserved