Mechanical Properties Metric English Comments
Tensile Strength at Break 18.2 MPa
2640 psi
ASTM D638
LyondellBasell Alathon® M5562 High Density Polyethylene
ApplicationsALATHON M 5562 is a copolymer with medium molecular weight distribution. This resin provides moderate stiffness, toughness and stress crack resistance. Typical applications include noz..
Tensile Strength at Break 18.2 MPa
2640 psi
ASTM D638
ITW Devcon Metal Repair Bronze Putty (BR), Bronze
Information provided by ITW Devcon
Tensile Strength at Break 18.2 MPa
2640 psi
Change in tensile strength in air after 168 hours at 277°F; ASTM D573
Teknor Apex Telcar® TL-8451 Thermoplastic Elastomer
Notes: RoHS Compliant Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Jacketing; Terminal Cable Jacketing; Undergrou..
Tensile Strength at Break 18.2 MPa
2640 psi
ASTM D412
UBE UBEPOL VCR303 Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C)
Description: UBEPOL-VCR is a new type of synthetic rubber system developed by UBE's original technology. UBEPOL-VCR consists of micro-dispersed syndiotactic 1,2-polybutadiene (SPB) with high mel..
Tensile Strength at Break 18.2 MPa
2640 psi
ASTM D638
Asahi Glass AFLAS® SP TFE/P/VdF Fluoroelastomer
AFLAS® SZ/SP are terpolymers containing tetrafluoroethylene, propylene, and a small amount of vinylidene fluoride used as a cure site monomer. This combination gives AFLAS® SZ/SP a good balance of..