Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 18.5 MPa | 2680 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible XV 1144 Polyvinyl Chloride, Flexible (PVC, Flexible) All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high .. |
|||
Tensile Strength at Break | 18.5 MPa | 2680 psi | ASTM D412 |
UBE UBEPOL BR150L Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C) Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE. |
|||
Tensile Strength at Break | 18.5 MPa | 2680 psi | ASTM D638 |
Asahi Glass AFLAS® 100H TFE/P Fluoroelastomer AFLAS® 100/150 fluoroelastomers are alternating copolymers of tetrafluoroethylene and propylene. They offer 1) excellent heat resistance, 2) exceptional chemical resistance especially to bases and .. |
|||
Tensile Strength at Break | 18.5 MPa | 2680 psi | |
Asahi Glass Fluon® PA1025Z 25% Glass Fiber, PTFE Filled Compound Fluon®PTFE FC has improved creep and wear resistance. A wide range of fillers such as glass fiber, graphite, bronze, carbon fiber are available. Information provided by Asahi Glass Company, Inc. |
|||
Tensile Strength at Break | 18.5 MPa | 2680 psi | |
Radici Radilene® R 30 IE 0 3036 B Low Density Polyethylene Shore hardness: 55 D (3s)Processable, recyclable, no charge and completely non-toxicApplication examples: coating of corrugated and non-corrugated pipe (conduit, plumbing pipe, steel pipe coating a.. |