Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | >= 27.58 MPa | >= 4000 psi | Sintered Molding; ASTM D4894-98a |
3M Dyneon™ TF 1641 PTFE Meets ASTM D4894 Type IV, Grade 2 resinMolding and ram extrusion powder very good free-flow propertiesGood metering propertiesGood mold filling behaviorGood electrical and mechanical propertiesVery .. |
|||
Tensile Strength at Break | >= 27.58 MPa | >= 4000 psi | Sintered Molding; ASTM D4894-98a |
3M Dyneon™ TF 1750 PTFE Meets ASTM D4894 Type IINon-free-flowing powder gradeVery fine particle sizeGood electrical and mechanical propertiesLow molding pressureUsed in large billet moldingExcellent for production of very .. |
|||
Tensile Strength at Break | >= 27.58 MPa | >= 4000 psi | Sintered Molding; ASTM D4894-98a |
3M Dyneon™ TF 1645 PTFE Meets ASTM D4894 Type IV, Grade 2 resinMolding and ram extrusion powder very good free-flow propertiesGood metering propertiesGood mold filling behaviorGood electrical and mechanical propertiesUsed .. |
|||
Tensile Strength at Break | >= 27.58 MPa | >= 4000 psi | Sintered Molding; ASTM D4894-98a |
3M Dyneon™ TF 1620 PTFE Meets ASTM D4894 Type IV, Grade 2 resinSemi-free-flowing compression molding powderHigh bulk densityGood for large billets and thin walled isostatic moldingsVery dense polymer structure, similar to .. |