Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 19.13 MPa | 2775 psi | JIS-K-6723 |
Denka VINYKON W4200 PVC, W grade for equipment cords, for heat resistance A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |