Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 283 - 324 MPa | 41000 - 47000 psi | Strip, Temper-Ex. Hard |
Lucas-Milhaupt BRAZE 999 Commercial Grade Fine Silver Commercial grade fine silver (99.90% minimum silver) is widely used in numerous electrical, electronic, and industrial applications, such as contacts, fuse elements, lead wires, battery plated, and .. |
|||
Tensile Strength at Break | 283 MPa @Temperature -40.0 °C |
41000 psi @Temperature -40.0 °F |
ASTM Test |
BASF Ultramid® 8233G HS 33% Glass Filled PA6 (Dry) Ultramid 8233G HS is a heat stabilized, 33% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. It is also.. |
|||
Tensile Strength at Break | 283 MPa @Temperature -40.0 °C |
41000 psi @Temperature -40.0 °F |
ISO Data |
BASF Ultramid® 8233G HS 33% Glass Filled PA6 (Dry) Ultramid 8233G HS is a heat stabilized, 33% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. It is also.. |