Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 1500 - 2000 MPa | 218000 - 290000 psi | |
Goodfellow Cobalt/Silicon/Boron/Manganese Alloy Information provided by Goodfellow.Composition Notes: Si + B content = 25 wt%. Fe+Mo content = 2 wt%. |
|||
Tensile Strength at Break | 1500 - 2000 MPa | 218000 - 290000 psi | |
Goodfellow Nickel 78/Boron 14/Silicon 8 Alloy Information provided by Goodfellow. |
|||
Tensile Strength at Break | 1500 - 2000 MPa | 218000 - 290000 psi | |
Goodfellow Nickel/Iron/Silicon/Boron Alloy Metallic glass (glassy alloy) or amorphous metal. Uses include soft magnetic applications, brazing, coating and as reinforcing fibers.Information provided by Goodfellow.Composition Notes: Si + B co.. |