Polymer Property : Tensile Strength at Break = 2930 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 20.2 MPa
2930 psi
ASTM D412
Teknor Apex APEX® 2585-H Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Good FlexibilityUses-General Purpose, ProfilesAppearance-Natural Color, OpaqueForms-PelletsProcessin..
Tensile Strength at Break 20.2 MPa
2930 psi
ASTM D3759
3M 420 Lead Foil Tape
Linered plasting tapeInformation provided by 3M