Polymer Property : Tensile Strength at Break = 2981 psi
Polymer Property :
Tensile Strength at Break =
2981 psi
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
20.55
MPa
2981
psi
ISO R 527
Stir SpA AF 91 (PVC)
Application: Flame insulation CEI 20-11 type R 2Information provided by STIR SpA