Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 2.06 MPa @Time 3.60e+6 sec |
299 psi @Time 1000 hour |
G-26, B, BH; ASTM D412 |
3M 4000 UV 5280 Marine Adhesive/Sealant Fast Cure 3M™ Marine Adhesive/Sealant 4000 UV is a one-part adhesive sealant that cures to form a firm, rubbery waterproof seal. Its flexibility allows for the dissipation of stress caused by shock, vibratio.. |
|||
Tensile Strength at Break | 2.06 MPa @Time 3.60e+6 sec |
299 psi @Time 1000 hour |
G-26, B, BH; ASTM D412 |
3M 4000 UV 6580 Marine Adhesive/Sealant Fast Cure 3M™ Marine Adhesive/Sealant 4000 UV is a one-part adhesive sealant that cures to form a firm, rubbery waterproof seal. Its flexibility allows for the dissipation of stress caused by shock, vibratio.. |
|||
Tensile Strength at Break | 2.06 MPa @Time 3.60e+6 sec |
299 psi @Time 1000 hour |
G-26, B, BH; ASTM D412 |
3M 4000 UV 6586 Marine Adhesive/Sealant Fast Cure 3M™ Marine Adhesive/Sealant 4000 UV is a one-part adhesive sealant that cures to form a firm, rubbery waterproof seal. Its flexibility allows for the dissipation of stress caused by shock, vibratio.. |