Tensile Strength at Break 3.258 MPa
472.5 psi
Air at 158°F, 168 hr; ASTM D573
ExxonMobil Santoprene® 8291-55PA Thermoplastic Elastomer  (discontinued **)
A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to PA-6 and blends thereof for applications where hard/s..