Mechanical Properties Metric English Comments
Tensile Strength at Break 3.31 MPa

@Temperature 23.0 °C
480 psi

@Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7930-1001-00 Thermoplastic Elastomer (TPE)
Dynaflex™ G7930-1001-00 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Non-Slip Grip - Overmold Adhesion..
Tensile Strength at Break 3.31 MPa

@Temperature 23.0 °C
480 psi

@Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7930-9 NSFG Thermoplastic Elastomer (TPE)
Dynaflex™ G7930-9 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. - NSF 51 approved - FDA (see Notes) - Overmold Adhesion to Polypropylene - Soft To..
Tensile Strength at Break 3.31 MPa

@Temperature 23.0 °C
480 psi

@Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7930-9001-02 Thermoplastic Elastomer (TPE)
Dynaflex™ G7930-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Non-Slip Grip - Overmold Adhesion..
Tensile Strength at Break 3.31 MPa

@Temperature 23.0 °C
480 psi

@Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7930-1 NSFG Thermoplastic Elastomer (TPE)
Dynaflex™ G7930-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. - NSF 51 approved - FDA (see Notes) - Overmold Adhesion to Polypropylene - Soft To..
Tensile Strength at Break 3.31 MPa

@Temperature 23.0 °C
480 psi

@Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynalloy™ OBC 8100-N50 Thermoplastic Elastomer (TPE)
Dynalloy™ OBC8100-N50 is a TPE developed utilizing the unique rubber properties of Dow INFUSE™ Olefin Block Copolymers. The 8100 Series has been specifically developed for applications requiring t..
Tensile Strength at Break 3.31 MPa
480 psi
Abatron L060421-1 Heat-Resistant (-75~400°F) Non-Flammable Silicone Rubber
L060421-1 is a heat-resistant and non-flammable silicone rubber recommended as a potting compound for exceptional protection against thermal shock, vibration, moisture, ozone, dust, chemicals, and o..