Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength at Break = 3.38 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 3.38 MPa

@Temperature 23.0 °C
490 psi

@Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7640-9 (Black) Thermoplastic Elastomer (TPE)
Dynaflex™ G7640-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl..
Tensile Strength at Break 3.38 MPa

@Temperature 23.0 °C
490 psi

@Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7640-1 (Natural) Thermoplastic Elastomer (TPE)
Dynaflex™ G7640-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Non-Slip Grip - Overmold Adhe..
Tensile Strength at Break 3.38 MPa
490 psi
(20 in/min), Molded Properties; ASTM D638
ExxonMobil Escorene™ MV 02514 Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: MV 02514 is a high flow copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: ..