Polymer Property : Tensile Strength at Break = 300000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 2070 MPa
300000 psi
0°; RT
Greene Tweed Xycomp® 1001-01 PEEK, Carbon Fiber Filled
Greene, Tweeds Xycomp® engineered components offer a wider range of benefits than conventional thermoset resin systems because they rely on thermoplastic resins for their matrix. With specific st..