Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 255 - 303 MPa | 37000 - 44000 psi | Strip, Temper-Hard |
Lucas-Milhaupt BRAZE 999 Commercial Grade Fine Silver Commercial grade fine silver (99.90% minimum silver) is widely used in numerous electrical, electronic, and industrial applications, such as contacts, fuse elements, lead wires, battery plated, and .. |